MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Silver, Ag; Commercially Pure (UNS P07020)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Pure Element

Key Words: UNS P07020
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.49 g/cc0.3790 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 2525
Tensile Strength, Ultimate 125 MPa18100 psi
Tensile Strength, Yield 54.0 MPa
@Strain 0.2 %
7830 psi
@Strain 0.2 %
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %
Modulus of Elasticity 71.0 GPa10300 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000147 ohm-cm0.00000147 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.1 µm/m-°C10.6 µin/in-°F
Specific Heat Capacity 0.234 J/g-°C0.0559 BTU/lb-°F
Thermal Conductivity 419 W/m-K2910 BTU-in/hr-ft²-°F
Melting Point 961.78 °C1763.2 °F
Boiling Point 2162 °C3924 °F
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag >= 99.9 %>= 99.9 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag; Refined, ASTM 413 (UNS P07015)
Silver, Ag
Silver, Ag; Refined, ASTM 413 (UNS P07010)
Silver, CP Grade, 10% Cold Worked
Silver, CP Grade, 70% Cold Worked

MPAgS90 / 100384

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.