MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Magnesium AS21-F, Die Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Good strength, creep resistance to 150°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³Estimated
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5555500 kg load, 10 mm ball
Tensile Strength, Ultimate 221 MPa32000 psi
Tensile Strength, Yield 117 MPa17000 psi
Elongation at Break 13 %13 %in 50 mm
Tensile Modulus 45.0 GPa6530 ksiTypical Mg alloy
Compressive Yield Strength 117 MPa17000 psi
Poissons Ratio 0.350.35Estimated from similar Mg alloys.
Shear Modulus 17.0 GPa2470 ksiEstimated from similar Mg alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  26.0 µm/m-°C
@Temperature 0.000 - 100 °C
14.4 µin/in-°F
@Temperature 32.0 - 212 °F
Estimated from similar Mg alloys.
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.2 %2.2 %
Magnesium, Mg 96.7 %96.7 %As Remainder
Manganese, Mn >= 0.10 %>= 0.10 %
Silicon, Si 1.0 %1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AS41A-F, Die Cast
Magnesium AM60A-F, Die Cast
Magnesium AM100A-T4, Cast
Magnesium AM20-F, Die Cast
Magnesium AM50A-F, Die Cast

MMAS21F / 12306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.