MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Uses: CPI equipment, industrial components, plate frame heat exchangers.

Mechanical property data below is typical of annealed samples at room temperature.

Information provided by Allegheny Ludlum.

Key Words: ASTM B-265
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.52 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120120
Tensile Strength, Ultimate 345 MPa50000 psi
Tensile Strength, Yield 206 MPa
@Strain 0.2 %
29900 psi
@Strain 0.2 %
Elongation at Break 35 %35 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.030 %<= 0.030 %
Oxygen, O <= 0.18 %<= 0.18 %
Palladium, Pd 0.050 %0.050 %
Titanium, Ti >= 99.5 %>= 99.5 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402)
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)
ATI Allvac® Grade 12 UNS R53400 Titanium Alloy
ATI Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age

NLTIT17 / 18062

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.