System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyether Grade
Material Notes:
Information provided by Bayer Corporation, Plastics Division
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Key Words:
TPUR
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.08
g/cc
0.0390
lb/in³
ASTM D792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
87
87
ASTM D2240
Tensile Strength, Ultimate
31.0
MPa
4500
psi
ASTM D412
Tensile Strength, Yield
5.00
MPa
725
psi
50% Elongation; ASTM D412
Elongation at Break
425 %
425 %
ASTM D412
Flexural Modulus
0.0410
GPa
5.95
ksi
ASTM D790
Resilience
30
30
% Bayshore Resilience; ASTM D2632
Tear Strength
80.0
kN/m
456
pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles
60
60
H-18 Wheel, 1000 g load, ASTM D3489
Thermal Properties
Metric
English
Comments
Vicat Softening Point
50.0
°C
122
°F
Rate A; ASTM D1525
Glass Transition Temp, Tg
-55.0
°C
-67.0
°F
DMA
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Bayflex® 970 Polyether-based Polyurethane System, Density 34 pcf
PB1T21 / 26565
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.