MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Carbon Fiber Composite

Material Notes: VYNTEC® CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several oils. Datasheet is based on postcured test specimens.

Information provided by Sumitomo Bakelite North America, Inc.

Key Words: PF-(CF+CD)50
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.570 g/cc0.0206 lb/in³ISO 60
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %ISO 62
Linear Mold Shrinkage 0.00020 cm/cm0.00020 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 108 MPa15700 psiISO 527-1
Elongation at Break 0.40 %0.40 %ISO 527-1
Tensile Modulus 31.0 GPa4500 ksiISO 527-1
Flexural Strength 239 MPa34700 psiISO 178
Flexural Modulus 28.0 GPa4060 ksiISO 178
Compressive Strength 200 MPa29000 psiISO 604
Charpy Impact Unnotched 1.09 J/cm²5.19 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.280 J/cm²1.33 ft-lb/in²ISO 179-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 4.00 µm/m-°C2.22 µin/in-°FTMA
CTE, linear, Transverse to Flow 27.0 µm/m-°C15.0 µin/in-°FTMA
Deflection Temperature at 1.8 MPa (264 psi) >= 250 °C>= 482 °FISO 75 Af
Shrinkage 0.020 %0.020 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit Vyntec® CF8050 Carbon Fiber Reinforced Phenolic
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound

PVYNC944 / 142719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.