MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Goodfellow Niobium 99/Zirconium 1 Alloy
Categories: Metal; Nonferrous Metal; Niobium Alloy; Refractory Metal

Material Notes: High temperature alloy used in Sodium and Magnesium vapor lamp electrodes and for coating the inside of Stainless Steel 316 tubes to improve corrosion resistance. The alloy combines moderate strength with excellent fabrication properties and is used extensively in nuclear applications because it has a low thermal neutron absorption cross section, good corrosion resistance and good resistance to radiation damage.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.59 g/cc0.310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 65 - 14065 - 140kg(f)/mm²
Tensile Strength at Break 330 - 620 MPa47900 - 89900 psi
Elongation at Break 5.0 - 30 %5.0 - 30 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 2399 °C4350 °F
 
Component Elements PropertiesMetricEnglishComments
Niobium, Nb (Columbium, Cb) 99 %99 %
Zirconium, Zr 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Niobium 56/Titanium 44 Alloy
ATI Wah Chang Nb/Nb Alloy C-103
Niobium Nb-1Zr (Wah Chang WC-1Zr; Fansteel 80), Commercial Grade
Niobium, Nb; Unalloyed CG (UNS R04210; UNS R04211)
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer

NGOODF202 / 16272

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.