MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 222.0-T65, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Key Words: Aluminium 222.0-T65; UNS A02220; AA222.0-T65; Al222.0-T65
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.95 g/cc0.107 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125 - 155125 - 155AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 177177Estimated from Brinell Hardness.
Hardness, Rockwell A 5151Estimated from Brinell Hardness.
Hardness, Rockwell B 8484Estimated from Brinell Hardness.
Hardness, Vickers 162162Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 276 MPa>= 40000 psiAA
Tensile Modulus 71.0 GPa10300 ksiEstimated
Poissons Ratio 0.330.33Estimated
Machinability 90 %90 %0-100 Scale (100=best)
Shear Modulus 26.7 GPa3870 ksiEstimated
Shear Strength 167 MPa24200 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000520 ohm-cm0.00000520 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  22.1 µm/m-°C
@Temperature 20.0 - 100 °C
12.3 µin/in-°F
@Temperature 68.0 - 212 °F
 23.6 µm/m-°C
@Temperature 20.0 - 300 °C
13.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 130 W/m-K902 BTU-in/hr-ft²-°F
Melting Point 518 - 624 °C964 - 1160 °F
Solidus 518 °C964 °F
Liquidus 624 °C1160 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 84 %84 %As remainder
Copper, Cu 9.2 - 10.7 %9.2 - 10.7 %
Iron, Fe 1.5 %1.5 %
Magnesium, Mg 0.15 - 0.35 %0.15 - 0.35 %
Manganese, Mn 0.50 %0.50 %
Nickel, Ni 0.50 %0.50 %
Silicon, Si 2.0 %2.0 %
Titanium, Ti 0.25 %0.25 %
Zinc, Zn 0.80 %0.80 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 201.0-T6 Casting Alloy
Aluminum 208.0-T6, Permanent Mold Cast
Aluminum 204.0-T6, Permanent Mold Cast, Precipitation Treatment 12 h at 180°C (360°F)
Aluminum 206.0-T7 Casting Alloy
Aluminum 204.0-T6, Permanent Mold Cast, Precipitation Treatment 12 h at 140°C (285°F)

MAC2220T65 / 9798

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.