ISO Shortname: ISO 7391-PC,MP,(,,)-09-9 MVR (300 °C/1.2 kg) 11 cm³/10 min; impact modified; medium viscosity; easy release; injection molding - melt temperature 280 - 320 °C; available in opaque colors only