MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 7500 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component file E40654. 07500 is available in black or red color.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.520 g/cc0.0188 lb/in³ASTM D1895
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.36 %0.36 %ASTM D570
Linear Mold Shrinkage 0.0109 cm/cm0.0109 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8787ASTM D785
Tensile Strength, Ultimate 62.0 MPa8990 psiASTM D638
Elongation at Break 0.87 %0.87 %ASTM D638
Tensile Modulus 8.10 GPa1170 ksiASTM D638
Flexural Strength 86.0 MPa12500 psiASTM D790
Flexural Modulus 7.00 GPa1020 ksiASTM D790
Compressive Strength 212 MPa30700 psiASTM D695
Izod Impact, Notched 0.193 J/cm0.362 ft-lb/inASTM D256
Charpy Impact, Notched 0.186 J/cm²0.885 ft-lb/in²ASTM D256
Impact 115115J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+13 ohm-cm5.00e+13 ohm-cmASTM D247
Dielectric Constant 4.34.3ASTM D150
Dielectric Strength 11.3 kV/mm287 kV/inShort Time; ASTM D149
Dissipation Factor 0.0440.044ASTM D150
Arc Resistance 120 sec120 secASTM D495
Comparative Tracking Index 150 V150 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 43.0 µm/m-°C
@Temperature 40.0 - 130 °C
23.9 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 197 °C387 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 151 °C304 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Shrinkage 0.35 %0.35 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PA6 GF25 FR HS L 25% Glass Filled
RTP Company RTP 1499 X 130922 A Polyethersulfone (PES); Electrically Conductive - Carbon Nanotube - High Purity
Kraton® G2705 GU (SEBS) Compound

PLEM41 / 50721

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.