MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EMS-Grivory Grilamid® LCL-3 H anthracite PA12-CF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties:
  • high stiffness and strength
  • very low density
  • excellent notched impact resistance also at low temperatures
  • low creep
  • high heat distortion temperatures
  • very low moisture absorption
  • very good dimensional stability and little warpage
  • excellent UV-resistance
  • electrically conductive
  • low wear and coefficient of friction
The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement of highest performance. Grilamid LCL-3H anthracite is used in the following market segments:
  • sports and leisure articles
  • mechanical engineering
  • household and appliances
The carbon-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³Dry; ISO 1183
Water Absorption 1.1 %1.1 %Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Sim. to ISO 62
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 135 MPa19600 psiConditioned; ISO 2039-1
Tensile Strength at Break 250 MPa36300 psiConditioned; ISO 527-1/-2
Elongation at Break 1.7 %1.7 %Conditioned; ISO 527-1/-2
Tensile Modulus 19.0 GPa2760 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 ohm-cm100 ohm-cmConditioned; IEC 60093
Surface Resistance 50 ohm50 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °C320 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Exterior
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesLong Fiber Reinforced
Special CharacteristicsAnti-static
 Improved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LC-3H black PA12-CF30
Avient Edgetek® NN-30CF/000 FR V0 Nylon 6/6, Carbon Fiber Reinforced
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
EMS-Grivory Grilon® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45
Overview of materials for Nylon 66, 10% Carbon Fiber Filled

PGRH067 / 156776

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.