MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP Technology Windform® XT 2.0 IMG Carbon Fiber Reinforced Nylon PA 12 for Injection Molding
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: Windform XT2.0 IMG is a PA12 based nylon material reinforced with carbon fiber, for high performance production. XT2.0 IMG is 100% recycled and built from high quality SLS materials . Our formulation features premium performances ranking from high stiffness and resistance to shock to extreme details accuracy even with thin walls. Its excellent properties makes it ideal for demanding application in a variety of industries such as automotive, transport, e-mobility, agriculture, robotics and industrial design.

Applications:

  • High Quality injection molded parts preserving same performances of prototypes realized in AM with Windform XT2.0
  • Automotive, e-mobility, transport: rigid parts for interiors and exteriors, bearings, bushings, gears, snap-fit components, fixtures
  • Electrical: enclosures and housings
  • Agriculture:planting and harvesting components, seed trays, greenhouse parts
  • Consumer and household goods:packaging and design objects
  • Industrial products:furniture parts, fixtures and tooling

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.182 g/cc0.04270 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 94 - 9694 - 96UNI EN ISO 868
Tensile Strength at Break 74.70 MPa10830 psiUNI EN ISO 527-1
Elongation at Break 14.3 %14.3 %UNI EN ISO 527-1
Tensile Modulus 7.547 GPa1095 ksiUNI EN ISO 527-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 179.3 °C354.7 °FISO 11357-2
 
Descriptive Properties
ColorBlack
Specific Tensile Modulus6309[MPa/(g/cc)], Tensile Modulus per density unit
Specific Tensile Strength63.2[MPa/(g/cc)], UTS per density unit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRPT30c / 318858

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.