MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kumho-Sunny HW600FR AES
Categories: Polymer; Thermoplastic; AES Polymer

Material Notes: HW600FR is general purpose flame retardant AES resin. The flame retardant rate is 1.5mm-V0. It has high weather resistance properties. HW600FR is mainly used in electric and electron and outside parts needing flame resistance.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Maximum Moisture Content 0.0500.050
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Flexural Strength 55.0 MPa7980 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 1.80 J/cm
@Thickness 3.20 mm
3.37 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 86.0 °C187 °FASTM D1525
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 200 °C374 - 392 °F
Middle Barrel Temperature 190 - 200 °C374 - 392 °F
Front Barrel Temperature 190 - 210 °C374 - 410 °F
Nozzle Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Back Pressure 1.00 - 5.00 MPa145 - 725 psi
Screw Speed 30 - 70 rpm30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN110 / 280962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.