MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

60-40 Soft Solder (60 Sn-40Pb) (UNS L13601)
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Key Words: ASTM B32 (60B)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.52 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1616
Hardness, Vickers 1616Cast; wide variation possible
Tensile Strength, Ultimate 53.0 MPa7690 psibulk solder; wide variation is possible.
Elongation at Break 30 - 60 %30 - 60 %
Tensile Modulus 30.0 GPa4350 ksibulk solder
 30.0 GPa4350 ksibulk solder
Poissons Ratio 0.400.40
Shear Modulus 11.0 GPa1600 ksiCalculated
Shear Strength 39.0 MPa5660 psi
Izod Impact 20.0 J14.8 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00001499 ohm-cm0.00001499 ohm-cm
Critical Magnetic Field Strength, Oersted 83.283.2mT at 1.3 K
Critical Superconducting Temperature 7.05 K7.05 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 37.0 J/g15.9 BTU/lb
CTE, linear 24.0 µm/m-°C
@Temperature 15.0 - 110 °C
13.3 µin/in-°F
@Temperature 59.0 - 230 °F
Specific Heat Capacity 0.173 J/g-°C0.0413 BTU/lb-°F
Thermal Conductivity 49.8 W/m-K346 BTU-in/hr-ft²-°F
Melting Point 183 - 190 °C361 - 374 °F
Solidus 183 °C361 °F
Liquidus 190 °C374 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb 0.20 - 0.50 %0.20 - 0.50 %
Arsenic, As <= 0.030 %<= 0.030 %
Bismuth, Bi <= 0.25 %<= 0.25 %
Copper, Cu <= 0.080 %<= 0.080 %
Iron, Fe <= 0.020 %<= 0.020 %
Lead, Pb 40 %40 %
Tin, Sn 60 %60 %
Zinc, Zn <= 0.0050 %<= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
60-40 Soft Solder (60 Sn-40Pb) Tin-Lead Soft Solder (UNS L13600)
Lead-Tin-Lithium-Calcium Alloy (UNS L51790)
Pig Tin (UNS L13002)
Pig Tin (UNS L13008)
Tin-Lead Eutectic Solder (63Sn-37Pb), Drop Solder (UNS L13630)

MLS13601 / 205641

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.