MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röchling GLASTHERM S Insulation Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature exceeds 425°F. Grade S is asbestos-free and rugged to withstand rough handling during installation. Suited to rubber molding industry.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.84 g/cc0.0665 lb/in³ASTM D-792
Water Absorption 0.40 %0.40 %% by wt.; ASTM D-570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9494ASTM D-785
Flexural Strength 124 MPa18000 psiASTM D-790
Compressive Strength  68.9 MPa
@Temperature 288 °C
10000 psi
@Temperature 550 °F
ASTM D-695
 79.3 MPa
@Temperature 200 °C
11500 psi
@Temperature 392 °F
ASTM D-695
 110 MPa
@Temperature 150 °C
16000 psi
@Temperature 302 °F
ASTM D-695
 310 MPa
@Temperature 23.9 °C
45000 psi
@Temperature 75.0 °F
ASTM D-695
Compressive Modulus 12.4 GPa1800 ksiASTM D-695
Izod Impact, Notched 4.27 J/cm8.00 ft-lb/inASTM D-256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 2.00 kV/mm50.8 kV/inPerpendicular S/T in Air; ASTM D-149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 20.0 °C
6.11 µin/in-°F
@Temperature 68.0 °F
Across Surface; ASTM D-696
 70.2 µm/m-°C
@Temperature 20.0 °C
39.0 µin/in-°F
@Temperature 68.0 °F
Across Thickness; ASTM D-696
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°FASTM C-177
Maximum Service Temperature, Air 218 °C425 °F
Flammability, UL94 HB
@Thickness 23.9 mm
HB
@Thickness 0.940 in
 
Descriptive Properties
Standard ColorTan
Thickness Tolerance in± 0.002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Uninhibited Naval brass, UNS C46400, H01 (8%) Temper 25 mm rod/bar
Gilding Copper, UNS C21000, Hard Temper
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass

PGLASW5 / 41939

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.