MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei XYRON™ C443V Polyphenylene Ether + PS, 30% Glass/Mineral Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Carbon Filler; Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: Product Description: Modified PPE; 30% Filler reinforced Flame retardant V-1; Electrically Conductive, Stiffness High, Warpage Low

Availability: Africa & Middle East; Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber\Carbon Fiber, 30% Filler by Weight

Features: Electrically Conductive; Flame Retardant; Halogen Free; Low Warpage

Processing Method: Injection Molding

Part Marking Code (ISO 11469): PPE+PS-(GF+CF)30FR(40)

Information provided by Asahi Kasei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/in150x150x2 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 73.1 MPa10600 psiISO 527
Elongation at Break 1.0 %1.0 %ISO 527
Flexural Strength 117 MPa17000 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Charpy Impact, Notched 0.399 J/cm²
@Thickness 4.00 mm
1.90 ft-lb/in²
@Thickness 0.157 in
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1000 ohm-cm100 - 1000 ohm-cmIEC 60093
Surface Resistance 100 - 1000 ohm100 - 1000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature -30.0 - 65.0 °C
7.80 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359-2
CTE, linear, Transverse to Flow 52.2 µm/m-°C
@Temperature -30.0 - 65.0 °C
29.0 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-1
@Thickness 1.52 mm
V-1
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 300 °C482 - 572 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASAHJ003 / 310696

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.