MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Beryllium-Copper Casting Alloy 275C, UNS C82800, TB00 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, Permanent Mold, Plaster, and Sand.

Applications: Bearings and molds for plastic parts.

Test specimen: TB00 temper, solution treated at 790-800°C.

Key Words: BeCu; beryllium copper 275C, CA 828, FED QQ-C-390, MIL-T-16243, MIL-C-19464 (Class IV), ICI-Cu-2-10788
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.09 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8585
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 240 MPa
@Strain 0.2 %
34800 psi
@Strain 0.2 %
Elongation at Break 10 %10 %In 50 mm
Modulus of Elasticity 133 GPa19300 ksi
Poissons Ratio 0.300.30
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 51.0 GPa7400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000958 ohm-cm
@Temperature 20.0 °C
0.0000958 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 95.0 W/m-K
@Temperature 20.0 °C
659 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 855 °C1570 °FIncipient
 860 - 930 °C1580 - 1710 °F
Solidus 835 °C1540 °F
Liquidus 930 °C1710 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Solution Temperature 790 - 800 °C1450 - 1470 °F
Aging Temperature 345 °C653 °F
Casting Temperature 965 - 1040 °C1770 - 1900 °FHeavy castings
 1040 - 1150 °C1900 - 2100 °FLight castings
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.15 %<= 0.15 %
Beryllium, Be 2.5 - 2.75 %2.5 - 2.75 %
Chromium, Cr <= 0.10 %<= 0.10 %
Cobalt, Co 0.37 - 0.70 %0.37 - 0.70 %
Copper, Cu >= 94.8 %>= 94.8 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.020 %<= 0.020 %
Nickel, Ni <= 0.20 %<= 0.20 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Tin, Sn <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium-Copper Casting Alloy 275C, UNS C82800, Cast and Aged
Beryllium-Copper Casting Alloy 275C, UNS C82800, TF00 Temper
Beryllium-Copper Casting Alloy 245C, UNS C82600, TB00 Temper
Beryllium-Copper Casting Alloy 275C, UNS C82800, As-Cast
Beryllium Copper 21C UNS C82510 Casting Alloy Solution Treated and Aged

MC82800b4 / 11897

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.