MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced

Material Notes: Natural Color Polyphenylene Sulfide Alloy

Xtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and rigidity along with excellent flow in thin-walled parts, low flash characteristics, and fast cycle times. Xtel™ XK2240 can be easily molded in conventional injection molding equipment utilizing water heated molds.

Comments: Test specimen molding conditions: Stock Temperature, 280-305°C; Mold Temperature, 80°C; ASTM Values Converted to SI Units

Data provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/in102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inMeasured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 195 MPa28300 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Yield Strength 275 MPa39900 psiASTM D790
Flexural Modulus 13.0 GPa1890 ksiASTM D790
Compressive Yield Strength 225 MPa32600 psiASTM D695
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
Izod Impact, Unnotched 8.00 J/cm15.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
 4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm686 kV/inASTM D149
Dissipation Factor  0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
ASTM D150
 0.030
@Frequency 1000 Hz
0.030
@Frequency 1000 Hz
ASTM D150
Arc Resistance 116 sec116 secASTM D495
Comparative Tracking Index 275 V275 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear  22.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
12.2 µin/in-°F
@Temperature -58.0 - 122 °F
Axial; ASTM E831
 39.0 µm/m-°C
@Temperature 100 - 200 °C
21.7 µin/in-°F
@Temperature 212 - 392 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow  63.0 µm/m-°C
@Temperature 20.0 °C
35.0 µin/in-°F
@Temperature 68.0 °F
ASTM E831
 110 µm/m-°C
@Temperature 100 - 200 °C
61.1 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy

PCHEVY46 / 20609

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.