Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent filler acceptance makes Elvaloy® 1125 AC suitable for highly filled compounds. Elvaloy® 1125 AC is easily processed on standard equipment used for low-density polyethylene. Information provided by DuPont. This former DuPont product line is now a Dow product line. |