Medium Molecular Weight. Excellent processability, good tear and impact strength, good stiffness, excellent compatibility with LDPE and LLDPE, excellent drawdown, good moisture barrier properties. Applications: Multiwall liner, gas flush poultry bags, mailing envelopes, heavy duty shipping sacks, fresh cut produce packaging, coextrusions. MatWeb has a separate entry for the resin using high stalk extrusion. This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture. |