MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Styropor® F 295-N Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)

Remarks: Production of flame-retardant foams displaying low post-shrinkage

Applications: Blocks, thin-walled molded parts.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 - 1.05 g/cc1.02 - 1.05 g/cc
Density 0.00310 g/cc0.000112 lb/in³Pentane Blowing Agent Vapor (Heavier than air)
 0.600 g/cc0.0217 lb/in³
Bead Size 1.00 - 2.30 mm0.0394 - 0.0906 in
Vapor Pressure 0.685 bar
@Temperature 25.0 °C
514 torr
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 70.0 °C158 °Fapprox
Decomposition Temperature >= 220 °C>= 428 °F
Flash Point >= -56.0 °C>= -68.8 °FPentane Blowing Agent
Ignition Temperature 285 °C545 °FPentane Blowing Agent; DIN 51794
 
Descriptive Properties
ColorWhite
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Expanded Polystyrene (EPS)
Aclo Accutech Polypropylene Homopolymer HP0339C20L1 Calcium Reinforced
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)
BASF Styropor® F 215 L-N Expandable Polystyrene
BASF Styropor® F 215 T-N Expandable Polystyrene

PBASG0186 / 131819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.