MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

High-Chromium Iron, corrosion resistant
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron

Material Notes: Martensite, austenite matrix structure as cast.

Key Words: Corrosion resistant high-chromium iron, martensitic, austenitic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.31 - 7.50 g/cc0.264 - 0.271 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 250 - 740250 - 740
Tensile Strength 205 - 830 MPa29700 - 120000 psi
Compressive Strength 690 MPa100000 psi
Charpy Impact 0.100 - 3.00 J0.0738 - 2.21 ft-lbStandard Charpy
Charpy Impact, Unnotched 27.0 - 47.0 J
@Diameter 30.5 mm
19.9 - 34.7 ft-lb
@Diameter 1.20 in
Test bar broken on 6 in (152 mm) supports
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.40 - 9.90 µm/m-°C
@Temperature 21.0 °C
5.22 - 5.50 µin/in-°F
@Temperature 69.8 °F
average
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.2 - 4.0 %1.2 - 4.0 %
Chromium, Cr 12 - 35 %12 - 35 %
Copper, Cu <= 3.0 %<= 3.0 %
Iron, Fe 58 %58 %
Manganese, Mn 0.30 - 1.5 %0.30 - 1.5 %
Molybdenum, Mo <= 4.0 %<= 4.0 %
Nickel, Ni <= 5.0 %<= 5.0 %
Phosphorus, P <= 0.15 %<= 0.15 %
Silicon, Si 0.50 - 3.0 %0.50 - 3.0 %
Sulfur, S <= 0.15 %<= 0.15 %
 
Descriptive Properties
Transverse Breaking Load910 to 1590 kgAs-cast 30.5 mm (1.2 in.) diameter bar; 457 mm (18 in.) span
Transverse Deflection1.5 to 3.8 mm (0.06 to 0.15 in)As-cast 30.5 mm (1.2 in.) diameter bar; 457 mm (18 in.) span

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
Overview of materials for Alloy Cast Iron
Overview of materials for Cast Iron
High-Nickel Ductile Iron, corrosion resistant
High-Chromium Iron, heat-resistant gray iron

MAFEA4 / 10234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.