MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1000
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Center or intermediate test location.

Martensitic, precipitation hardening (maraging) stainless steel.

Key Words: UNS S13800, 13-8Mo, 13-8PH, 13-8 PH, 13/8 Mo, 13/8Mo, 13/8PH, 13/8 PH, AMS 5629, AMS 5840, ASME SA705 (XM-13), ASTM A564 (XM-13), ASTM A693 (XM-13), ASTM A705 (XM-13); PH 13-8 Mo; Precipitation Hardening
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1480 MPa215000 psi
Tensile Strength, Yield 1415 MPa
@Strain 0.2 %
205200 psi
@Strain 0.2 %
Elongation at Break 13 %13 %in 50 mm
Modulus of Elasticity 221 GPa32100 ksi
Machinability 35 - 40 %35 - 40 %Based on 100% machinability for AISI 1212 steel.
 35 - 40 %35 - 40 %Based on 100% machinability for AISI 1212 steel.
Charpy Impact 54.0 J39.8 ft-lb
 5.00 J
@Temperature -195 °C
3.69 ft-lb
@Temperature -319 °F
 9.00 J
@Temperature -140 °C
6.64 ft-lb
@Temperature -220 °F
 16.0 J
@Temperature -115 °C
11.8 ft-lb
@Temperature -175 °F
 22.0 J
@Temperature -73.0 °C
16.2 ft-lb
@Temperature -99.4 °F
 27.0 J
@Temperature -54.0 °C
19.9 ft-lb
@Temperature -65.2 °F
 41.0 J
@Temperature 0.000 °C
30.2 ft-lb
@Temperature 32.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000100 ohm-cm
@Temperature 25.0 °C
0.000100 ohm-cm
@Temperature 77.0 °F
in Condition A.
 0.000100 ohm-cm
@Temperature 100 °C
0.000100 ohm-cm
@Temperature 212 °F
in Condition A.
 0.000100 ohm-cm
@Temperature 200 °C
0.000100 ohm-cm
@Temperature 392 °F
in Condition A.
 0.000110 ohm-cm
@Temperature 315 °C
0.000110 ohm-cm
@Temperature 599 °F
in Condition A.
 0.000110 ohm-cm
@Temperature 425 °C
0.000110 ohm-cm
@Temperature 797 °F
in Condition A.
 0.000110 ohm-cm
@Temperature 540 °C
0.000110 ohm-cm
@Temperature 1000 °F
in Condition A.
 0.000110 ohm-cm
@Temperature 595 °C
0.000110 ohm-cm
@Temperature 1100 °F
in Condition A.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 21.0 - 95.0 °C
5.89 µin/in-°F
@Temperature 69.8 - 203 °F
 10.8 µm/m-°C
@Temperature 21.0 - 205 °C
6.00 µin/in-°F
@Temperature 69.8 - 401 °F
 11.2 µm/m-°C
@Temperature 21.0 - 315 °C
6.22 µin/in-°F
@Temperature 69.8 - 599 °F
 11.9 µm/m-°C
@Temperature 21.0 - 540 °C
6.61 µin/in-°F
@Temperature 69.8 - 1000 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  14.0 W/m-K
@Temperature 100 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 212 °F
in Condition A
 15.7 W/m-K
@Temperature 200 °C
109 BTU-in/hr-ft²-°F
@Temperature 392 °F
in Condition A
 17.8 W/m-K
@Temperature 315 °C
124 BTU-in/hr-ft²-°F
@Temperature 599 °F
in Condition A
 20.4 W/m-K
@Temperature 425 °C
142 BTU-in/hr-ft²-°F
@Temperature 797 °F
in Condition A
 22.3 W/m-K
@Temperature 540 °C
155 BTU-in/hr-ft²-°F
@Temperature 1000 °F
in Condition A
 22.5 W/m-K
@Temperature 595 °C
156 BTU-in/hr-ft²-°F
@Temperature 1100 °F
in Condition A
Melting Point 1405 - 1440 °C2561 - 2620 °F
Solidus 1405 °C2561 °F
Liquidus 1440 °C2620 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.90 - 1.35 %0.90 - 1.35 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 12.25 - 13.25 %12.25 - 13.25 %
Iron, Fe 76 %76 %
Manganese, Mn <= 0.10 %<= 0.10 %
Molybdenum, Mo 2.0 - 2.5 %2.0 - 2.5 %
Nickel, Ni 7.5 - 8.5 %7.5 - 8.5 %
Nitrogen, N <= 0.010 %<= 0.010 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.0080 %<= 0.0080 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition RH950
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H950
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1050
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1100
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1150M

MQM138C / 13475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.