MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Red Gum Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.440 g/cc0.0159 lb/in³Oven Dry Weight/Unseasoned Volume
 0.801 g/cc0.0289 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2300 N517 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2800 N629 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 3.52 MPa510 psiPerpendicular to Grain*
Modulus of Rupture 0.0469 GPa6.80 ksiStatic Bending*
Flexural Yield Strength 25.5 MPa3700 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 7.93 GPa1150 ksiStatic Bending*
Compressive Strength 3.17 MPa460 psiPerpendicular to Grain*
 16.3 MPa2360 psiParallel to Grain*
 19.6 MPa2840 psiMax Crushing Strength Parallel to Grain*
Shear Strength 7.38 MPa1070 psiParallel to Grain*
Impact 3.93.9in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 1000010000psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00558 J/cm³0.810 in-lb/in³Static Bending*
Work to Maximum Load 0.0648 J/cm³9.40 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Shrinkage 5.2 %5.2 %Radial; Unseasoned to Oven Dry*
 9.9 %9.9 %Tangential; Unseasoned to Oven Dry*
 15 %15 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Red Maple Wood
American Pignut Hickory Wood
American Black Gum (Black Tupelo) Wood
American Pecan Hickory Wood
North American Black Willow Wood

PTSA060 / 71244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.