MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sciengy ES-SGC101S21 PPS/PTFE, 10% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: ES-SGC101S21 is a 10% carbon fiber reinforced PPS & PTFE compound specially formulated to have a low coefficient of friction for use in low surface friction and wear applications, specially lower wear performance

Information provided by Shandong Sciengy New Materials Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Water Absorption at Saturation 0.040 %0.040 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inGB/T 15585
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inGB/T 15585
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 125 MPa18100 psiISO 527
Elongation at Break 1.2 %1.2 %ISO 527
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²IS0 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 330 °C554 - 626 °FInjection molding; ISO 294
Mold Temperature 120 - 160 °C248 - 320 °FInjection molding; ISO 294
Drying Temperature 150 °C
@Time 10800 sec
302 °F
@Time 3.00 hour
Injection Pressure 30.0 - 100 MPa4350 - 14500 psi
 
Descriptive Properties
Limit in-cylinder retention time300?/60min
 320?/30min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCIE047 / 297094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.