MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Riteflex® 447 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 447 is a nominal 47 Shore D thermoplastic polyester polyester elastomer with a high melting point and excellent mechanical properties.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 0.50 %
@Temperature 22.8 °C
0.50 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.013 - 0.018 cm/cm0.013 - 0.018 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 240 °C
15 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiISO 527-1/2
Elongation at Break 800 %800 %ISO 527-1/2
Tensile Modulus 0.0950 GPa13.8 ksi50mm/min; ISO 527-2/1A
Flexural Strength 6.00 MPa870 psiISO 178
 4.00 MPa
@Strain 3.5 %
580 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.0900 GPa13.1 ksiISO 178
Resilience 5959Bayshore, %
Izod Impact, Notched (ISO)  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact, Notched NBNBISO 179/1eA
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+12 ohm-cm4.00e+12 ohm-cmASTM D257
 4.00e+14 ohm-cm4.00e+14 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohm2.00e+15 ohmIEC 60093
Dielectric Constant 4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 12.2 kV/mm310 kV/inshort term; ASTM D149
 13.0 kV/mm330 kV/inIEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VASTM D3638
 >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 220 µm/m-°C122 µin/in-°FISO 11359-2
Melting Point 212 °C414 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FISO 75-1, -2
Flammability, UL94 HBHB
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 425 TPC, Unfilled
Celanese Riteflex® 435 TPC, Unfilled
Celanese Riteflex® 265B TPC
Celanese Riteflex® 440 TPC, Unfilled

PHCQ450 / 178905

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.