MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Traid Villarroya TVH® TV 6061-T6 Extruded (AA 6061) Aluminum alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes:
  • Medium mechanical properties
  • Great resistance to corrosion
  • Good weldability properties
Industry Applications:
  • Components for railroad
  • Nautical
  • Defense and aviation
  • Stressed structures

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 110110
Tensile Strength at Break 360 MPa52200 psiRm
Tensile Strength, Yield 320 MPa46400 psiRp 0.2
Elongation at Break 11 %11 %
Modulus of Elasticity 69.0 GPa10000 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000037 ohm-cm0.0000037 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.5 µm/m-°C13.1 µin/in-°F
Thermal Conductivity 173 W/m-K1200 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 96 - 98.61 %96 - 98.61 %As Remainder
Chromium, Cr 0.040 - 0.35 %0.040 - 0.35 %
Copper, Cu 0.15 - 0.40 %0.15 - 0.40 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.80 - 1.2 %0.80 - 1.2 %
Manganese, Mn <= 0.15 %<= 0.15 %
Silicon, Si 0.40 - 0.80 %0.40 - 0.80 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.25 %<= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NTRAID944 / 318911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.