MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) ST 730°C; overage 580°C
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Excellent mechanical properties up to 315 °C. High strength and high toughness. Deep hardenability, excellent creep stability, excellent forgability.

Applications: Airframe applications, milling, forgings

Forms typically available: Billet, bar and plate

5 other heat treatments of this alloy are in MatWeb.

Key Words: KS 10-2-3; Ti-10-2-3; TIMETAL 10-2-3
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.65 g/cc0.168 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 980 MPa142000 psi
Tensile Strength, Yield 940 MPa136000 psi
Elongation at Break 22 %
@Thickness 15.0 mm
22 %
@Thickness 0.591 in
in 5 cm
Reduction of Area 56 %56 %
Modulus of Elasticity 102 GPa14800 ksi
Ultimate Bearing Strength 2000 MPa290000 psie/D = 2
Bearing Yield Strength 1560 MPa226000 psie/D = 2
Poissons Ratio 0.330.33Typical for beta titanium alloy.
Fatigue Strength  890 MPa
@# of Cycles 1.00e+6
129000 psi
@# of Cycles 1.00e+6
unnotched
 910 MPa
@# of Cycles 10000
132000 psi
@# of Cycles 10000
Fracture Toughness 102 MPa-m½92.8 ksi-in½K(IC)
Shear Modulus 41.0 GPa5950 ksi
Charpy Impact 30.0 J22.1 ft-lbV-notch; avg. of longitudinal and transverse
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cmEstimated from similar high-V-stabilized beta titanium alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.60 µm/m-°C
@Temperature 425 - 1150 °C
4.78 µin/in-°F
@Temperature 797 - 2100 °F
 9.70 µm/m-°C
@Temperature 20.0 - 425 °C
5.39 µin/in-°F
@Temperature 68.0 - 797 °F
average
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity 7.80 W/m-K54.1 BTU-in/hr-ft²-°FEstimated from similar high-V-stabilized beta titanium alloys.
Maximum Service Temperature, Air 315 °C599 °F
Beta Transus 760 °C1400 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.6 - 3.4 %2.6 - 3.4 %
Carbon, C <= 0.050 %<= 0.050 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe 1.6 - 2.2 %1.6 - 2.2 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.13 %<= 0.13 %
Titanium, Ti 82.855 - 86.8 %82.855 - 86.8 %As Balance; Elemental Composition per ASTM B265
Vanadium, V 9.0 - 11 %9.0 - 11 %
 
Descriptive Properties
Crystal StructurebccBeta, predominant
 cphAlpha

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) ST 760°C, Aged 385°C
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) Solution Treated 850°C (1560°F)
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) ST 760°C; Age 525°C (980°F)
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3) ST 815°C, Anneal 620°C
Titanium Ti-10V-2Fe-3Al (Ti 10-2-3), Anneal 1 hr. 760°C

MTB023 / 14147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.