MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 7701 Epoxy - Quartz Fiber 8 Harness Satin Fabric Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Composite with Quartz Fiber Reinforced 8 Harness Satin Fabric. CYCOM® 7701 resin is a 250°F (121°C) curing epoxy resin designed for use in structural laminates and honeycomb core sandwich panels for aircraft exteriors. In the prepreg form it has excellent drape and tack. CYCOM 7701 was created for autoclave fabrication; however, it can also be press molded and vacuum bag cured. The recommended lay-up procedure for CYCOM 7701 epoxy resin is L-3 or L-6. The recommended cure procedure is C-6 or C-7.

Features & Benefits:

  • 250°F (121°C) cure
  • 200°F (93°C) dry service temperature
  • Laminate and sandwich panel usage
  • Self-extinguishing and solvent resistant
  • Self-adhesive to honeycomb core
  • Autoclave, press mold or vacuum bag processing
  • Shelf life 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications: Structural laminates and honeycomb core sandwich panels for aircraft exteriors

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 545 - 558 MPa
@Temperature 24.0 °C
79000 - 81000 psi
@Temperature 75.2 °F
Tensile Modulus 25.0 - 26.0 GPa
@Temperature 24.0 °C
3630 - 3770 ksi
@Temperature 75.2 °F
Compressive Strength 448 - 462 MPa
@Temperature 24.0 °C
65000 - 67000 psi
@Temperature 75.2 °F
Compressive Modulus 24.0 - 26.0 GPa
@Temperature 24.0 °C
3480 - 3770 ksi
@Temperature 75.2 °F
Shear Strength 26.9 - 28.3 MPa
@Thickness 610 mm
3900 - 4100 psi
@Thickness 24.0 in
Interlaminar
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °Fdry
 
Processing PropertiesMetricEnglishComments
Processing Temperature 121 °C250 °FCure Temperature
Shelf Life  0.333 Month
@Temperature 22.0 °C
0.333 Month
@Temperature 71.6 °F
 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 7701 Epoxy - Crowfoot Satin Fabric Composite
Solvay CYCOM® 7701 Epoxy - 8 Harness Satin Fabric Composite

PCYTED083b / 233302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.