MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 20% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.68 g/cc0.0452 - 0.0607 lb/in³Average value: 1.53 g/cc Grade Count:48
Filler Content 15.0 - 20.0 %15.0 - 20.0 %Average value: 18.2 % Grade Count:11
Water Absorption 0.0300 - 0.800 %0.0300 - 0.800 %Average value: 0.362 % Grade Count:19
Moisture Absorption at Equilibrium 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.180 % Grade Count:5
Water Absorption at Saturation 0.200 - 0.850 %0.200 - 0.850 %Average value: 0.736 % Grade Count:7
Linear Mold Shrinkage 0.00300 - 0.0245 cm/cm0.00300 - 0.0245 in/inAverage value: 0.00827 cm/cm Grade Count:39
Linear Mold Shrinkage, Transverse 0.00900 - 0.0265 cm/cm0.00900 - 0.0265 in/inAverage value: 0.0139 cm/cm Grade Count:11
Melt Flow 1.10 - 12.0 g/10 min1.10 - 12.0 g/10 minAverage value: 6.85 g/10 min Grade Count:17
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 82.0 - 89.082.0 - 89.0Average value: 84.4 Grade Count:5
Hardness, Rockwell R 82.0 - 11082.0 - 110Average value: 95.6 Grade Count:8
Tensile Strength, Ultimate 52.0 - 140 MPa7540 - 20300 psiAverage value: 89.0 MPa Grade Count:35
 32.0 - 50.0 MPa
@Temperature 60.0 - 120 °C
4640 - 7250 psi
@Temperature 140 - 248 °F
Average value: 41.7 MPa Grade Count:1
Tensile Strength, Yield 46.0 - 117 MPa6670 - 17000 psiAverage value: 87.8 MPa Grade Count:14
Elongation at Break 1.50 - 15.0 %1.50 - 15.0 %Average value: 4.45 % Grade Count:45
Modulus of Elasticity 3.40 - 12.0 GPa493 - 1740 ksiAverage value: 6.28 GPa Grade Count:25
Flexural Yield Strength 50.0 - 210 MPa7250 - 30500 psiAverage value: 131 MPa Grade Count:36
Flexural Modulus 3.20 - 9.10 GPa464 - 1320 ksiAverage value: 5.65 GPa Grade Count:42
 2.40 - 3.90 GPa
@Temperature 60.0 - 120 °C
348 - 566 ksi
@Temperature 140 - 248 °F
Average value: 3.13 GPa Grade Count:1
Izod Impact, Notched 0.100 - 0.801 J/cm0.187 - 1.50 ft-lb/inAverage value: 0.572 J/cm Grade Count:24
Izod Impact, Unnotched 3.74 - 5.87 J/cm7.00 - 11.0 ft-lb/inAverage value: 5.04 J/cm Grade Count:8
Izod Impact, Notched (ISO) 5.00 - 7.00 kJ/m²2.38 - 3.33 ft-lb/in²Average value: 5.76 kJ/m² Grade Count:7
 6.00 - 6.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 - 6.00 J/cm²9.52 - 28.6 ft-lb/in²Average value: 4.09 J/cm² Grade Count:10
 4.00 - 5.00 J/cm²
@Temperature -30.0 - -30.0 °C
19.0 - 23.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:4
Charpy Impact, Notched 0.300 - 0.950 J/cm²1.43 - 4.52 ft-lb/in²Average value: 0.569 J/cm² Grade Count:24
 0.300 - 0.800 J/cm²
@Temperature -30.0 - -30.0 °C
1.43 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.450 J/cm² Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 4000 - 1.00e+17 ohm-cm4000 - 1.00e+17 ohm-cmAverage value: 5.19e+15 ohm-cm Grade Count:24
Surface Resistance 1600 - 5.00e+16 ohm1600 - 5.00e+16 ohmAverage value: 4.07e+15 ohm Grade Count:17
Dielectric Constant 3.90 - 4.503.90 - 4.50Average value: 4.15 Grade Count:7
Dielectric Strength 16.0 - 35.0 kV/mm406 - 889 kV/inAverage value: 23.2 kV/mm Grade Count:12
Dissipation Factor 0.00300 - 0.02000.00300 - 0.0200Average value: 0.00785 Grade Count:7
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 589 V Grade Count:9
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 100 µm/m-°C16.7 - 55.6 µin/in-°FAverage value: 51.9 µm/m-°C Grade Count:16
CTE, linear, Transverse to Flow 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FAverage value: 93.0 µm/m-°C Grade Count:9
Melting Point 160 - 180 °C320 - 356 °FAverage value: 167 °C Grade Count:22
Deflection Temperature at 0.46 MPa (66 psi) 161 - 176 °C322 - 348 °FAverage value: 165 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 110 - 163 °C230 - 325 °FAverage value: 152 °C Grade Count:41
Vicat Softening Point 120 - 163 °C248 - 325 °FAverage value: 154 °C Grade Count:6
Flammability, UL94 HBHBGrade Count:35
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 230 °C176 - 446 °FAverage value: 169 °C Grade Count:17
Die Temperature 190 - 210 °C374 - 410 °FAverage value: 199 °C Grade Count:7
Melt Temperature 170 - 230 °C338 - 446 °FAverage value: 193 °C Grade Count:21
Mold Temperature 45.0 - 121 °C113 - 250 °FAverage value: 86.9 °C Grade Count:24
Injection Velocity 20.0 - 50.0 mm/sec0.787 - 1.97 in/secAverage value: 35.0 mm/sec Grade Count:3
Drying Temperature 80.0 - 121 °C176 - 250 °FAverage value: 98.0 °C Grade Count:25
Moisture Content 0.150 - 0.200 %0.150 - 0.200 %Average value: 0.159 % Grade Count:11
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:4
Injection Pressure 30.0 - 140 MPa4350 - 20300 psiAverage value: 84.2 MPa Grade Count:19

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
Overview of materials for Acetal Copolymer, Glass Bead Filled

O1252 / 77841

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.