Physical Properties | Metric | English | Comments |
---|
Density | 1.43 g/cc | 0.0517 lb/in³ |
Water Absorption | 0.80 % @Time 86400 sec | 0.80 % @Time 24.0 hour |
Moisture Absorption at Equilibrium | 0.90 % | 0.90 % |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 110 MPa | 16000 psi |
| 133 MPa | 19300 psi |
Elongation at Break | 2.2 % | 2.2 % |
| 2.5 % | 2.5 % |
Tensile Modulus | 8.90 GPa | 1290 ksi |
| 10.7 GPa | 1550 ksi |
Flexural Strength | 169 MPa | 24500 psi |
| 197 MPa | 28600 psi |
Flexural Modulus | 8.10 GPa | 1170 ksi |
| 10.4 GPa | 1510 ksi |
Izod Impact, Notched (ISO) | 7.80 kJ/m² @Temperature 23.0 °C | 3.71 ft-lb/in² @Temperature 73.4 °F |
| 8.10 kJ/m² @Temperature -30.0 °C | 3.85 ft-lb/in² @Temperature -22.0 °F |
| 8.50 kJ/m² @Temperature -40.0 °C | 4.04 ft-lb/in² @Temperature -40.0 °F |
| 8.80 kJ/m² @Temperature -30.0 °C | 4.19 ft-lb/in² @Temperature -22.0 °F |
| 9.00 kJ/m² @Temperature -40.0 °C | 4.28 ft-lb/in² @Temperature -40.0 °F |
| 9.00 kJ/m² @Temperature 23.0 °C | 4.28 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -40.0 °C | 24.3 ft-lb/in² @Temperature -40.0 °F |
| 5.20 J/cm² @Temperature -40.0 °C | 24.7 ft-lb/in² @Temperature -40.0 °F |
| 5.30 J/cm² @Temperature -30.0 °C | 25.2 ft-lb/in² @Temperature -22.0 °F |
| 5.60 J/cm² @Temperature -30.0 °C | 26.6 ft-lb/in² @Temperature -22.0 °F |
| 5.90 J/cm² @Temperature 23.0 °C | 28.1 ft-lb/in² @Temperature 73.4 °F |
| 6.10 J/cm² @Temperature 23.0 °C | 29.0 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 0.870 J/cm² @Temperature 23.0 °C | 4.14 ft-lb/in² @Temperature 73.4 °F |
| 0.910 J/cm² @Temperature -40.0 °C | 4.33 ft-lb/in² @Temperature -40.0 °F |
| 0.910 J/cm² @Temperature -30.0 °C | 4.33 ft-lb/in² @Temperature -22.0 °F |
| 0.910 J/cm² @Temperature -30.0 °C | 4.33 ft-lb/in² @Temperature -22.0 °F |
| 0.920 J/cm² @Temperature -40.0 °C | 4.38 ft-lb/in² @Temperature -40.0 °F |
| 0.990 J/cm² @Temperature 23.0 °C | 4.71 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm | 660 kV/in @Thickness 0.0394 in |
| 26.0 kV/mm @Thickness 1.00 mm | 660 kV/in @Thickness 0.0394 in |
Comparative Tracking Index | 600 V @Thickness 3.00 mm | 600 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec |
| >= 120 sec | >= 120 sec |
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs |
| >= 120 arcs | >= 120 arcs |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 259 °C | 498 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 257 °C | 495 °F |
| 257 °C | 495 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 238 °C | 460 °F |
| 239 °C | 462 °F |
UL RTI, Electrical | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 110 °C @Thickness 0.750 mm | 230 °F @Thickness 0.0295 in |
| 110 °C @Thickness 3.00 mm | 230 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
Flammability, UL94 | V-0 @Thickness 0.400 mm | V-0 @Thickness 0.0157 in |
| V-0 @Thickness 0.750 mm | V-0 @Thickness 0.0295 in |
| V-0 @Thickness 3.00 mm | V-0 @Thickness 0.118 in |
Oxygen Index | 35 % | 35 % |
Glow Wire Ignition Temperature | 725 °C @Thickness 0.400 mm | 1340 °F @Thickness 0.0157 in |
| 725 °C @Thickness 0.750 mm | 1340 °F @Thickness 0.0295 in |
| 750 °C @Thickness 3.00 mm | 1380 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 960 °C @Thickness 0.400 mm | 1760 °F @Thickness 0.0157 in |
| 960 °C @Thickness 0.750 mm | 1760 °F @Thickness 0.0295 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 265 - 275 °C | 509 - 527 °F |
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F |
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F |
Melt Temperature | 270 - 280 °C | 518 - 536 °F |
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 hour | 4.00 hour |
Moisture Content | 0.25 % | 0.25 % |
|
Descriptive Properties |
---|
Additive | Flame Retarding Agent |
| Heat Stabilizer |
| Release agent |
Appearance | Natural Color |
Features | Flame Retardant |
| Halogen Content, None |
Forms | Pellets |
Processing Method | Injection Molding |
Railway Classification | HL3 |
| HL3 |
Region | North America, Europe |
Smoke Density, Ds Max | 97 |
Smoke Toxicity, CITNLP | 0.47 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.