MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ascend Performance Materials HiDura™ D0MP NT0805 PA612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: HiDura™ D0MP NT0805 is a nucleated, lubricated and low viscosity PA612 molding grade. It exhibits excellent flow, crystallization rate and release making it suitable for injection molding of thin parts (i.e. cable ties, battery seals, etc). It exhibits low moisture absorption, good chemical resistance and dimensional stability. PA612 offers a unique balance of thermal, mechanical and physical properties.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³DAM; ISO 1183
Water Absorption 0.37 %
@Time 86400 sec
0.37 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %1.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
@Thickness 2.00 mm
0.020 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 57.0 MPa8270 psi50% RH; ISO 527-2
 66.0 MPa9570 psiDAM; ISO 527-2
Elongation at Break 21 %21 %DAM; ISO 527-2
 62 %62 %50% RH; ISO 527-2
Tensile Modulus 1.80 GPa261 ksi50% RH; ISO 527-2
 2.40 GPa348 ksiDAM; ISO 527-2
Flexural Strength 44.0 MPa6380 psi50% RH; ISO 178
 70.0 MPa10200 psiDAM; ISO 178
Flexural Modulus 1.70 GPa247 ksi50% RH; ISO 178
 2.30 GPa334 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  3.30 kJ/m²
@Temperature 23.0 °C
1.57 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 3.40 kJ/m²
@Temperature -30.0 °C
1.62 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 3.50 kJ/m²
@Temperature -40.0 °C
1.67 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.40 kJ/m²
@Temperature -40.0 °C
2.09 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 4.40 kJ/m²
@Temperature -30.0 °C
2.09 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 4.70 kJ/m²
@Temperature 23.0 °C
2.24 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.280 J/cm²
@Temperature -40.0 °C
1.33 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.300 J/cm²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.320 J/cm²
@Temperature 23.0 °C
1.52 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.360 J/cm²
@Temperature -30.0 °C
1.71 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.470 J/cm²
@Temperature 23.0 °C
2.24 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 31.0 kV/mm
@Thickness 1.00 mm
787 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 148 °C298 °FUnannealed; 50% RH; ISO 75-2/B
 151 °C304 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 235 - 290 °C455 - 554 °FInjection
Mold Temperature 50.0 - 90.0 °C122 - 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection
Moisture Content 0.15 %0.15 %Injection
 
Descriptive Properties
AdditiveLubricant
AppearanceNatural Color
FeaturesAbrasion Resistance
 Chemical Resistant
 Excellent Processability
 Fast Molding Cycle
 Good Dimensional Stability
 Good Flow
 Good Mold Release
 High Flow
 Low Viscosity
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9001 / 287542

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.