MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thickness is not less than 3mm.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Water Absorption <= 0.50 %<= 0.50 %ISO 62
Linear Mold Shrinkage 0.0016 cm/cm0.0016 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 12.0 MPa
@Temperature 22.0 °C
1740 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Tensile Strength, Yield 12.0 MPa
@Temperature 22.0 °C
1740 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Modulus of Elasticity 6.00 GPa870 ksi25 mm flat samples, compression molded; ISO 527-4
Flexural Strength 30.0 MPa
@Temperature 22.0 °C
4350 psi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 6.00 GPa
@Temperature 22.0 °C
870 ksi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.300.30
Shear Modulus 2.30 GPa334 ksiin plane
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°FISO 11359-2
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 240 °C>= 464 °FISO 75-2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 170 °C338 °FISO 11357-2
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 35 %35 %ISO 4589-2
Glow Wire Flammability Index 960 °C1760 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 145 - 165 °C293 - 329 °FCompression molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP
Polynt BMC 1150 Bulk Molding Compound ARC Ablation

PMENZ029 / 100763

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.