MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poly Alloy Etoma™ ET1101 PP with Carbon Black
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Etoma ET1101 resin is a conductive compound based on polypropylene with carbon black. ET1101 resin has not only stable surface resistivity but high impact property. The formula of ET1101 is designed to general purpose application which is very easy to be processed.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 24.5 MPa3560 psiASTM D638
Elongation at Break 12 %12 %ASTM D638
Flexural Strength 36.3 MPa5260 psiASTM D790
Flexural Modulus 1.47 GPa213 ksiASTM D790
Izod Impact, Notched 5.39 J/cm10.1 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 10000 ohm - 1e+0510000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648
Shrinkage 1.2 - 1.5 %1.2 - 1.5 %ASTM D955
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 - 210 °C392 - 410 °F
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 205 - 225 °C401 - 437 °F
Nozzle Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 30.0 - 65.0 °C86.0 - 149 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY016 / 278295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.