MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Baystar™ 37120 Medium Density Polyethylene Sheet Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes: Characteristics:

  • Good processability
  • Excellent melt strength
  • Superior stress cracking resistance
  • Broad fusion range
  • ASTM D1248 – Type II, Class A, Category 5

Applications:

  • Landfill liners
  • Pond liners
  • Mining films
  • Geomembranes

Information provided by Bayport Polymers LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D-792
ESCR 100% Igepal® >= 1500 hour>= 1500 hourASTM D-1693
ESCR 10% Igepal® >= 1500 hour>= 1500 hourASTM D-1693
Oxidative Induction Time (OIT) >= 100 min>= 100 minASTM D-3895
High Load Melt Index 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.6 MPa2700 psiASTM D-638
Elongation at Break >= 700 %>= 700 %ASTM D-638
Flexural Modulus 0.800 GPa116 ksiASTM D-790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBAYST804 / 251111

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.