MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Hyflon® MFA® P6022 Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Hyflon® MFA® P6022 is a clear, semi-crystalline melt processable perfluorinated resin. Due to it characteristic free-flowing properties, it is designed for use in rotomolding and rotolining applications. Rotomolding is typically used to manufacture articles such as tanks, bottles and vessels whilst rotolining is used in coat pipes, fittings, valves and tanks. The product exhibits excellent chemical inertness, excellent thermal and flame resistance and very low surface energy. Additionally it shows excellent smooth surface finish, very low coefficient of friction and outstanding optical properties. Main features of Hyflon® MFA® P6022 include:
  • Excellent flowability
  • Excellent chemical inertness
  • Outstanding surface finish
  • Excellent thermal resistance
  • Very low coefficient of friction

Availability:

  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
Features:
  • Good Surface Finish
  • Good Thermal Stabilty
  • Low Friction
  • Opticals
  • Semi Crystalline
Uses:
  • Coating Applications
Forms: Powder

Processing Method: Coating

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.16 g/cc0.0780 lb/in³ASTM D792
Particle Size 300 µm300 µm
Melt Flow 2.0 - 5.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
2.0 - 5.0 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 285 °C545 °FASTM D4591
 
Descriptive Properties
AppearanceClear/Transparent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Hyflon® MFA® P6310 Perfluoropolymer

PSOLVAY522 / 218250

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.