MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems Inconel 601 Washers and Studs
Categories: Ceramic; Oxide; Metal; Ferrous Metal; Stainless Steel

Material Notes: Kao-Lok Anchors, Washers and Studs are a combination refractory and stainless steel designed to be used with Thermal Ceramics blanket wallpaper furnace linings. Kao-Lok Anchor Systems have been one of the preferred methods of installing ceramic fiber wallpaper lining systems for more than 30 years.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 1121 °C<= 2050 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 23 %23 %
Iron, Fe 69.385 - 69.4 %69.385 - 69.4 %balance
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 6.0 %6.0 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 304SS Washers and Studs
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 310 SS Washers and Studs
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 330 SS Washers and Studs
Overview of materials for AISI 4000 Series Steel

CMORF6487 / 203271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.