MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gold-Platinum Alloy (70Au-30Pt), Annealed 1000°C then Quenched
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 19.92 g/cc0.7197 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 114114
Hardness, Knoop 131131Estimated from Brinell
Hardness, Rockwell A 4040Estimated from Brinell
Hardness, Rockwell B 6464Estimated from Brinell
Hardness, Vickers 115115Estimated from Brinell
Modulus of Elasticity 113.8 GPa16510 ksiTypical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000340 ohm-cm0.0000340 ohm-cmTemperature Coefficient = 0.0059 nanoOhm-m/K between 0-1200 K
 
Thermal PropertiesMetricEnglishComments
Melting Point 1228 - 1450 °C2242 - 2640 °F
Solidus 1228 °C2242 °F
Liquidus 1450 °C2640 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 70 %70 %
Platinum, Pt 30 %30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Platinum Alloy
Gold-Platinum Alloy (70Au-30Pt), Typical
Gold-Platinum Alloy (70Au-30Pt), Hard (66% Reduction)
Gold-Platinum Alloy (70Au-30Pt), Annealed at 1095°C (2000°F) then Air-Cooled
Gold, Au; Refined, Wrought (UNS P00025)

MPAuP1 / 12543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.