MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 6020-T9
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resistance, good joining characteristics, and excellent response to anodizing.

Uses: Automotive transmission valves, brake pistons, air conditioning compressor pistons, CATV connectors, hinge pins, camera parts, tripod fittings.

Composition Notes: Composition information provided by the Aluminum Association and is not for design.

Data supplied by Alcoa.

Key Words: 6020-T9 Aluminium; UNS A96020; Al6020-T9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120120500 kg load/10 mm ball
Hardness, Knoop 150150Estimated from Brinell
Hardness, Rockwell A 46.846.8Estimated from Brinell
Hardness, Rockwell B 7575Estimated from Brinell
Hardness, Vickers 136136Estimated from Brinell
Tensile Strength, Ultimate >= 352 MPa>= 51100 psi
Tensile Strength, Yield >= 338 MPa>= 49000 psi
Elongation at Break 5.0 %5.0 %
Machinability 90 %90 %0-100 Scale (A=90; B=70; C=50; D=30; E=10)
Shear Strength 211 MPa30600 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000370 ohm-cm0.00000370 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
average
Thermal Conductivity 171 W/m-K1190 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 93.9 - 97.8 %93.9 - 97.8 %As remainder
Chromium, Cr <= 0.15 %<= 0.15 %
Copper, Cu 0.30 - 0.90 %0.30 - 0.90 %
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.05 %<= 0.05 %
Magnesium, Mg 0.60 - 1.2 %0.60 - 1.2 %
Manganese, Mn <= 0.35 %<= 0.35 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 0.40 - 0.90 %0.40 - 0.90 %
Tin, Sn 0.90 - 1.5 %0.90 - 1.5 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6020-T8
Aluminum 6020-T651
Aluminum 6005-T1
Aluminum 6009-T4
Aluminum 6009-T6

MA6020T9 / 133638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.