MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI KELON B FR H CET/05-V2 5% Mineral Filled, Heat-Stabilized Nylon 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Mineral Filled

Material Notes: Description: Kelon B series thermoplastics are Nylon 6 with mineral fillers. The most important feature of the Kelon series is their high dimensional stability. Unlike the corresponding glass fiber filled compounds, no differential shrinkage occurs; molded parts are therefore essentially free from deformation. General performance values are good; the various Kelon versions have different properties as regards finish, flowability, shrinkage, rigidity, and impact resistance. The Kelon's can be painted with no particular problem, even with on-line paint at 150°-160°C. The toughness of the product is improved by using elastomer; therefore, conditioning in water to improve impact strength is not required. Most of Kelon's are substantially stable to processing temperatures. When formulated with special flame-retardant halogen additives guaranteeing a higher resistance to temperature, they can be molded as the corresponding non self-extinguishing products. These products are free from PBDE (Polybromodiphenyl ether) and PBDF (Polybromodibenzofuran).

Specific Notes for this Material: UL94V-2 self-extinguishing, without halogens or phosphorus; low fume optical density and toxicity; 5% mineral fillers; heat-stabilized; excellent flowability; excellent electrical properties.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inLATI
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 79.0 MPa11500 psiISO 527
Flexural Modulus 3.50 GPa508 ksiASTM D790
Izod Impact, Notched 0.340 J/cm
@Temperature 23.0 °C
0.637 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched 4.30 J/cm²
@Temperature 23.0 °C
20.5 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D648
Vicat Softening Point 203 °C397 °F50°C/h 50N; ISO 306
Flammability, UL94 V-2
@Thickness 0.710 mm
V-2
@Thickness 0.0280 in
Glow Wire Test  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 - 100 °C176 - 212 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATI011 / 50009

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.