MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zr-2.5Nb Zirconium Alloy, Nuclear Grade
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: Characteristics:
  • Higher strength than Zircaloys
  • High corrosion resistance to super-heated water, yet lower than the Zircaloys
  • Forms a stable, dense, self-healing oxide layer
  • Highly anisotropic

Applications: Pressure tubes in heavy water reactors

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant.

Key Words: UNS R60901, UNS R60902
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.44 g/cc0.233 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 150 - 500150 - 500
Tensile Strength, Ultimate >= 448 MPa>= 65000 psi
Tensile Strength, Yield >= 310 MPa
@Strain 0.2 %
>= 45000 psi
@Strain 0.2 %
Elongation at Break 20 %20 %in 50 mm
Modulus of Elasticity 97.9 GPa14200 ksi
Poissons Ratio 0.330.33
Shear Modulus 34.5 GPa5000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000550 ohm-cm0.0000550 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.30 µm/m-°C
@Temperature 25.0 °C
3.50 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 0.285 J/g-°C0.0681 BTU/lb-°F
Thermal Conductivity 17.1 W/m-K119 BTU-in/hr-ft²-°F
Melting Point 1840 °C3340 °F
Boiling Point 4380 °C7920 °F
 
Component Elements PropertiesMetricEnglishComments
Niobium, Nb (Columbium, Cb) 2.6 %2.6 %
Oxygen, O 0.14 %0.14 %
Zirconium, Zr 97.5 %97.5 %
 
Descriptive Properties
Alpha plus Beta Phase Crystal Structurehcp + bcc954°C
Beta Phase Crystal Structurebcc> 854°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Grade 705 Zirconium (Zr-2.5Nb)
Zircaloy-4 Zirconium Alloy
Grade 706 Zirconium (Zr-2.5Nb)
Reactor Grade Zirconium
Zircaloy-2 Zirconium Alloy

MZRN30 / 14577

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.