MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. The Cell Classification was determined using the notched Izod test with injection molded samples.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 797915 sec; ASTM D2240
Tensile Strength, Yield 42.1 MPa6110 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.48 GPa360 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.48 GPa360 ksiASTM D790
Izod Impact, Notched  10.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
18.7 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
 11.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
 11.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy  53.4 J/cm
@Temperature 23.0 °C
0.100 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 53.4 J/cm
@Temperature 23.0 °C
0.100 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C37.2 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.3 °C
@Thickness 3.18 mm
164 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 0.9195 mm
V-0
@Thickness 0.03620 in
All Colors
 V-0
@Thickness 0.749 mm
V-0
@Thickness 0.0295 in
ALL; UL 94
 5VA
@Thickness 1.90 mm
5VA
@Thickness 0.0748 in
ALL; UL 94
 5VA
@Thickness 1.58 mm
5VA
@Thickness 0.0622 in
All Colors
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
Agency RatingsNSF 51
Automotive SpecificationsGM GM7001M (PVC)
Ease of SizingExcellent
FeaturesGood Dimensional Stability
 Good Melt Strength
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16344ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Beltline Moldings
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80530 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80520 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 81520 Polyvinyl Chloride, Rigid

PH0POL0096 / 144665

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.