MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registered trademark of Dow Chemical Company.

Key Words: Fiberglass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM D572
Water Absorption 0.20 %0.20 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5555
Tensile Strength, Ultimate 70.0 MPa10200 psi
Flexural Strength 155 MPa22500 psi
Compressive Strength 207 MPa30000 psi
Izod Impact, Notched 4.30 J/cm8.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.0 kV/mm406 kV/inPerpendicular (ASTM D149), in Oil
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haysite HCR-196 Corrosion Resistant Vinyl Ester/Glass Sheet
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC

PHAY33 / 45639

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.