MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vanadium Carbide, VC
Categories: Ceramic; Carbide

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.71 g/cc0.206 lb/in³theoretical
Molecular Weight 62.953 g/mol62.953 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 9191at RT
Vickers Microhardness 29502950
Modulus of Elasticity 268 - 420 GPa38900 - 60900 ksiat RT
Compressive Strength 607 MPa88000 psiat RT
Poissons Ratio 0.220.22at RT
Shear Modulus 157 GPa22800 ksiat RT
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.20 µm/m-°C
@Temperature 20.0 °C
4.00 µin/in-°F
@Temperature 68.0 °F
Melting Point 2730 °C4950 °F
Solidus 2655 °C4811 °F
Liquidus 2810 °C5090 °F
 
Descriptive Properties
ColorBlack
Crystal StructureCubicNaCl Structure

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Tantalum Carbide, TaC
Tungsten Carbide, W2C
Titanium Carbide, TiC
Chromium Carbide, Cr3C2

BCVC1A / 164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.