MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polystyrene, Heat Resistant Grade
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.19 g/cc0.0376 - 0.0430 lb/in³Average value: 1.05 g/cc Grade Count:109
Water Absorption 0.000 - 0.100 %0.000 - 0.100 %Average value: 0.0433 % Grade Count:21
Moisture Absorption at Equilibrium 0.100 %0.100 %Average value: 0.100 % Grade Count:6
Water Absorption at Saturation 0.100 %0.100 %Average value: 0.100 % Grade Count:5
Maximum Moisture Content 0.01000.0100Average value: 0.0100 Grade Count:4
Linear Mold Shrinkage 0.00200 - 0.0114 cm/cm0.00200 - 0.0114 in/inAverage value: 0.00561 cm/cm Grade Count:90
Melt Flow 1.00 - 120 g/10 min1.00 - 120 g/10 minAverage value: 7.49 g/10 min Grade Count:113
Spiral Flow 43.0 - 62.0 cm
@Temperature 220 - 220 °C
16.9 - 24.4 in
@Temperature 428 - 428 °F
Average value: 51.9 cm Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 40.0 - 11040.0 - 110Average value: 101 Grade Count:34
Hardness, Rockwell M 45.0 - 78.045.0 - 78.0Average value: 74.3 Grade Count:22
Hardness, Rockwell R 91.0 - 12191.0 - 121Average value: 105 Grade Count:11
Ball Indentation Hardness 81.0 - 150 MPa11700 - 21800 psiAverage value: 144 MPa Grade Count:12
Tensile Strength, Ultimate 22.0 - 62.0 MPa3190 - 8990 psiAverage value: 47.1 MPa Grade Count:84
 18.0 - 18.0 MPa
@Temperature 60.0 - 60.0 °C
2610 - 2610 psi
@Temperature 140 - 140 °F
Average value: 18.0 MPa Grade Count:1
Tensile Strength, Yield 20.0 - 59.0 MPa2900 - 8560 psiAverage value: 45.9 MPa Grade Count:51
Elongation at Break 1.80 - 60.0 %1.80 - 60.0 %Average value: 9.16 % Grade Count:102
Elongation at Yield 1.50 - 3.00 %1.50 - 3.00 %Average value: 2.15 % Grade Count:4
Modulus of Elasticity 1.79 - 3.38 GPa260 - 490 ksiAverage value: 2.97 GPa Grade Count:89
Flexural Yield Strength 39.0 - 106 MPa5660 - 15400 psiAverage value: 80.6 MPa Grade Count:73
Flexural Modulus 1.50 - 3.45 GPa218 - 500 ksiAverage value: 3.02 GPa Grade Count:90
 1.90 - 1.90 GPa
@Temperature 60.0 - 60.0 °C
276 - 276 ksi
@Temperature 140 - 140 °F
Average value: 1.90 GPa Grade Count:1
Izod Impact, Notched 0.0981 - 1.30 J/cm0.184 - 2.44 ft-lb/inAverage value: 0.280 J/cm Grade Count:71
 0.400 - 0.500 J/cm
@Temperature -40.0 - -20.0 °C
0.749 - 0.937 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 0.168 J/cm Grade Count:1
 0.0980665 - 0.0980665 J/cm
@Temperature -30.0 - -30.0 °C
0.183719 - 0.183719 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.168 J/cm Grade Count:4
 0.0980665 - 0.0980665 J/cm
@Thickness 6.40 - 6.40 mm
0.183719 - 0.183719 ft-lb/in
@Thickness 0.252 - 0.252 in
Average value: 0.168 J/cm Grade Count:4
Izod Impact, Notched (ISO) 1.50 - 10.0 kJ/m²0.714 - 4.76 ft-lb/in²Average value: 6.33 kJ/m² Grade Count:12
Izod Impact, Unnotched (ISO) 7.00 kJ/m² - NB3.33 ft-lb/in² - NBAverage value: 10.2 kJ/m² Grade Count:6
Charpy Impact Unnotched 0.800 J/cm² - NB3.81 ft-lb/in² - NBAverage value: 1.69 J/cm² Grade Count:22
 3.50 - 3.50 J/cm²
@Temperature -40.0 - -20.0 °C
16.7 - 16.7 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 3.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.100 - 0.900 J/cm²0.476 - 4.28 ft-lb/in²Average value: 0.325 J/cm² Grade Count:6
Tensile Creep Modulus, 1 hour 3300 MPa479000 psiAverage value: 3300 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 2600 MPa377000 psiAverage value: 2600 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm1.00e+14 - 1.00e+18 ohm-cmAverage value: 2.12e+17 ohm-cm Grade Count:24
Surface Resistance 1.00e+13 - 1.00e+15 ohm1.00e+13 - 1.00e+15 ohmAverage value: 1.84e+14 ohm Grade Count:31
Dielectric Constant 2.00 - 2.702.00 - 2.70Average value: 2.40 Grade Count:35
Dielectric Strength 19.7 - 160 kV/mm500 - 4060 kV/inAverage value: 67.3 kV/mm Grade Count:47
Dissipation Factor 0.0000500 - 0.002000.0000500 - 0.00200Average value: 0.000460 Grade Count:17
Arc Resistance 120 - 180 sec120 - 180 secAverage value: 150 sec Grade Count:4
Comparative Tracking Index 250 - 350 V250 - 350 VAverage value: 308 V Grade Count:12
Hot Wire Ignition, HWI 7.00 - 30.0 sec7.00 - 30.0 secAverage value: 16.8 sec Grade Count:4
High Amp Arc Ignition, HAI 60.0 - 120 arcs60.0 - 120 arcsAverage value: 105 arcs Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 10.0 - 50.0 mm/min0.394 - 1.97 in/minAverage value: 32.7 mm/min Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 91.0 µm/m-°C27.8 - 50.6 µin/in-°FAverage value: 82.5 µm/m-°C Grade Count:55
Thermal Conductivity 0.123 - 0.170 W/m-K0.854 - 1.18 BTU-in/hr-ft²-°FAverage value: 0.159 W/m-K Grade Count:6
Hot Ball Pressure Test 90.0 °C194 °FAverage value: 90.0 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 82.8 - 187 °C181 - 369 °FAverage value: 96.1 °C Grade Count:49
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 175 °C167 - 347 °FAverage value: 89.4 °C Grade Count:101
Vicat Softening Point 85.0 - 210 °C185 - 410 °FAverage value: 104 °C Grade Count:112
Heat Distortion Temperature 78.9 - 98.9 °C174 - 210 °FAverage value: 84.8 °C Grade Count:10
Glass Transition Temp, Tg 89.0 - 104 °C192 - 219 °FAverage value: 98.0 °C Grade Count:7
UL RTI, Electrical 50.0 °C122 °FAverage value: 50.0 °C Grade Count:4
UL RTI, Mechanical with Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:4
UL RTI, Mechanical without Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:52
Oxygen Index 18.0 %18.0 %Average value: 18.0 % Grade Count:7
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 783 °C Grade Count:6
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.591.59Average value: 1.59 Grade Count:14
Optical Density 0.04600.0460Average value: 0.0460 Grade Count:14
Haze 1.00 %1.00 %Average value: 1.00 % Grade Count:3
Transmission, Visible 88.0 - 90.0 %88.0 - 90.0 %Average value: 89.2 % Grade Count:18
 
Processing PropertiesMetricEnglishComments
Processing Temperature 66.0 - 280 °C151 - 536 °FAverage value: 180 °C Grade Count:4
Nozzle Temperature 190 - 245 °C374 - 473 °FAverage value: 226 °C Grade Count:16
Die Temperature 199 - 232 °C390 - 450 °FAverage value: 216 °C Grade Count:12
Melt Temperature 138 - 280 °C280 - 536 °FAverage value: 212 °C Grade Count:53
Mold Temperature 10.0 - 82.0 °C50.0 - 180 °FAverage value: 52.9 °C Grade Count:29
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:3
Drying Temperature 60.0 - 80.0 °C140 - 176 °FAverage value: 76.2 °C Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Polystyrene, Flame Retardant
Overview of materials for Polystyrene, Extrusion Grade
Overview of materials for Polystyrene, Impact Modified
Overview of materials for Polystyrene, Transparent Grade

O4803 / 78413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.