MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chi Mei Acryrex® CM-205G Optical Grade PMMA Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded

Material Notes: Optical grade resin with low melt volume-flow rate. Applications: Widely used in optical extrusion applications. LGP raw material for 3D LCD TV and LCD monitor backlights.

ACRYREX® Optical PMMA Resin is made with 99% methyl methacrylate (MMA) and 1% additives. It features good cleanliness, weather resistance, heat resistance, transparency, and gloss. It also exhibits stable physical, chemical, optical, and electrical properties. ACRYREX® Optical Grade PMMA Resin is widely used in the application of optical grade light guide plates, lighting signage, and backlight modules.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 0.30 %
@Temperature 25.0 °C,
Time 86400 sec
0.30 %
@Temperature 77.0 °F,
Time 24.0 hour
ASTM D570
Melt Flow 1.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.8 g/10 min
@Load 8.38 lb,
Temperature 446 °F
Cond. I; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 97
@Thickness 6.35 mm
97
@Thickness 0.250 in
ASTM D785
Tensile Strength 70.6 MPa10200 psi1/8', 6mm/min; ASTM D638
Elongation at Break 5.0 %5.0 %1/8", 6mm/min; ASTM D638
Flexural Yield Strength 108 MPa15600 psi1/4", 2.8mm/min; ASTM D790
Izod Impact, Notched 0.196 J/cm
@Thickness 6.35 mm
0.367 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °F1/4", 120°C/hr; ASTM D648
Vicat Softening Point 113 °C235 °F1/8", 50°C/hr; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
UV Transmittance 92 %
@Thickness 3.17 mm
92 %
@Thickness 0.125 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHI9914 / 280799

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.