Daikin PTFE F-301 is a high molecular weight polytetrafluoroethylene fine powder resin for paste extrusion manufactured without the use of PFOA. F-301 has been specifically designed for the manufacture of un-sintered tapes, sintered tapes, coated wire and tubing at low to medium reduction ratios.Information provided by Daikin. |