Angst+Pfister APSOplast® POM-H POM homopolymer
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Homopolymer, Unreinforced
Material Notes:
POM homopolymer has a higher tensile strength, rigidity, hardness, creep resistance, and wear resistance than POM-C (copolymer).
Information provided by Angst + Pfister
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.42
g/cc
0.0513
lb/in³
DIN EN ISO 1183-1
Moisture Absorption
0.200 %
0.200 %
at saturation in standardized climate; DIN EN ISO 62
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
83
83
DIN EN ISO 868
Ball Indentation Hardness
160
MPa
23200
psi
DIN EN ISO 2039-1
Tensile Strength, Yield
75.0
MPa
10900
psi
50 mm/min; DIN EN ISO 527
Elongation at Break
30 %
30 %
50 mm/min; DIN EN ISO 527
Modulus of Elasticity
3.20
GPa
464
ksi
1 mm/min; DIN EN ISO 527
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
DIN EN ISO 179-1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
Dielectric Constant
3.8
3.8
IEC 60250
Dielectric Strength
25.0
kV/mm
635
kV/in
IEC 60243
Dielectric Loss Index
0.0020
0.0020
IEC 60250
Comparative Tracking Index
600
V
600
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
100
µm/m-°C
@Temperature 23.0 - 60.0 °C
55.6
µin/in-°F
@Temperature 73.4 - 140 °F
DIN 53752
Specific Heat Capacity
1.50
J/g-°C
0.359
BTU/lb-°F
Thermal Conductivity
0.310
W/m-K
2.15
BTU-in/hr-ft²-°F
Melting Point
175
°C
347
°F
ISO 11357-3
Maximum Service Temperature, Air
90.0
°C
194
°F
short term
150
°C
302
°F
long term
Deflection Temperature at 1.8 MPa (264 psi)
110
°C
230
°F
DIN EN ISO 75/A
Minimum Service Temperature, Air
-50.0
°C
-58.0
°F
Flammability, UL94
HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in
Descriptive Properties
Color
natural (white), black
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PANGP046 / 250544
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.