MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Starflam® PA6Z22V2D Nylon PA6 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Starflam PA6Z22V2D is an unfilled flame retardant PA6 resin for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³DAM; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 71.0 MPa10300 psiDAM; ISO 527-2
Elongation at Break 10 %10 %DAM; ISO 527-2
Tensile Modulus 3.40 GPa493 ksiDAM; ISO 527-2
Flexural Strength 91.0 MPa13200 psiDAM; ISO 178
Flexural Modulus 2.60 GPa377 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 6.40 kJ/m²
@Temperature 23.0 °C
3.05 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 108 kJ/m²
@Temperature 23.0 °C
51.4 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched 9.70 J/cm²
@Temperature 23.0 °C
46.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.520 J/cm²
@Temperature 23.0 °C
2.47 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °FDAM; ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FUnannealed; DAM; ISO 75-2/A
Glow Wire Flammability Index 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °FInjection
Middle Barrel Temperature 235 - 245 °C455 - 473 °FInjection
Front Barrel Temperature 240 - 260 °C464 - 500 °FInjection
Melt Temperature 240 - 260 °C464 - 500 °FInjection
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection
Drying Temperature 75.0 - 85.0 °C167 - 185 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA6 FR(30)
AppearanceNatural Color
FeaturesBromine Free
 Flame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8704 / 293365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.