MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Heat-Away™ 641-HT-EV Thermally Conductive Grease, Silver Filled, for High Vacuum Systems
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Heat-Away™ greases are ceramic and metal-filled systems that offer exceptional electrical and thermal properties up to 680ºF (360ºC). These materials are used in high power electronics, heat pipes, high vacuum systems, and other heat management applications.

Vendors: Aremco's Heat-Away™ greases are ceramic and metalfilled systems that offer exceptional electrical and thermal properties. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.20 g/cc4.20 g/cc
Solids Content 100 %100 %
Water Absorption 0.00 %0.00 %
Vapor Pressure  <= 5.33288e-018 bar
@Temperature 20.0 °C
<= 4.00e-15 torr
@Temperature 68.0 °F
 <= 2.67e-13 bar
@Temperature 100 °C
<= 2.00e-10 torr
@Temperature 212 °F
 <= 4.00e-10 bar
@Temperature 200 °C
<= 3.00e-7 torr
@Temperature 392 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00060 ohm-cm<= 0.00060 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 5.58 W/m-K38.7 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 360 °C680 °F
Minimum Service Temperature, Air -30.6 °C-23.0 °F
 
Descriptive Properties
Chemical ResistanceExcellent
ColorSilver
FillerSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM993d / 256042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.