MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 1180-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Key Words: Aluminium 1180-O; UNS A91180; AA1180-O; Al1180-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.705 g/cc0.09772 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1717500 kg load with 10 mm ball. Calculated value.
Tensile Strength, Ultimate 60.0 MPa8700 psi
Tensile Strength, Yield 20.0 MPa2900 psi
Elongation at Break 45 %45 %In 5 cm; Sample 1.6 mm thick
Tensile Modulus 67.0 GPa9720 ksiCompressive Modulus is about 2% higher
Poissons Ratio 0.330.33
Shear Modulus 25.0 GPa3630 ksiCalculated
Shear Strength 42.0 MPa6090 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000280 ohm-cm0.00000280 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 390 J/g168 BTU/lb
CTE, linear  23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
average
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 238 W/m-K1650 BTU-in/hr-ft²-°F
Melting Point 650 - 658 °C1200 - 1220 °F
Solidus 650 °C1200 °F
Liquidus 658 °C1220 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 99.8 %>= 99.8 %Specified
Copper, Cu <= 0.010 %<= 0.010 %
Gallium, Ga <= 0.030 %<= 0.030 %
Iron, Fe <= 0.090 %<= 0.090 %
Magnesium, Mg <= 0.020 %<= 0.020 %
Manganese, Mn <= 0.020 %<= 0.020 %
Silicon, Si <= 0.090 %<= 0.090 %
Titanium, Ti <= 0.020 %<= 0.020 %
Vanadium, V <= 0.050 %<= 0.050 %
Zinc, Zn <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1180-H18
Aluminum 1145-O
Aluminum 1199-O
Aluminum 1199-H18
Aluminum 1060-O

MA1180O / 8769

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.